KIRISH
1 Nikel 200 va 201 ni payvandlash uchun ishlatiladi. Titanning uglerod bilan reaksiyasi erkin uglerodning past darajasini saqlab qoladi va plomba metallini Nikel 201 bilan ishlatish imkonini beradi. Payvandlash metalliERNi-1ayniqsa ishqorlarda yaxshi korroziyaga chidamlilikka ega.
Umumiy nomlar: Oxford Alloy® 61 FM61
Standart: ASME SFA 5.14 UNS N02061 AWS 5.14 AWSERNi-1
KIMYOVIY TARKIBI (%)
| C | Si | Mn | S | P | Ni |
| ≤0.05 | 0,35-0,5 | ≤0.9 | ≤0.01 | ≤0.01 | ≥95.0 |
| Al | Ti | Fe | Cu | boshqalar | |
| ≤1.5 | 2.0-3.5 | ≤1.0 | ≤0.15 | <0.5 |
PAYVANDLASH PARAMETRLARI
| Jarayon | Diametri | Kuchlanishi | Amperaj | Gaz |
| TIG | .035″ (0.9 mm) .045″ (1.2 mm) 1/16 dyuym (1.6 mm) 3/32″ (2.4 mm) 1/8″ (3.2 mm) | 12-15 13-16 14-18 15-20 15-20 | 60-90 80-110 90-130 120-175 150-220 | 100% Argon 100% Argon 100% Argon 100% Argon 100% Argon |
| MIG | .035″ (0.9 mm) .045″ (1.2 mm) 1/16 dyuym (1.6 mm) | 26-29 28-32 29-33 | 150-190 180-220 200-250 | 75% Argon + 25% Geliy 75% Argon + 25% Geliy 75% Argon + 25% Geliy |
| arra | 3/32″ (2.4 mm) 1/8″ (3.2 mm) 5/32″ (4.0 mm) | 28-30 29-32 30-33 | 275-350 350-450 400-550 | Tegishli oqim ishlatilishi mumkin Tegishli oqim ishlatilishi mumkin Tegishli oqim ishlatilishi mumkin |
MEXANIK XUSUSIYATLAR
| Mustahkamlik chegarasi | 66 500 PSI | 460 MPA |
| Chidamlilik kuchi | 38 000 PSI | 260 MPA |
| Uzayish | 28% |
ARIZALAR
Nikel 200 va nikel 201 ni ulash uchun 1 ta nikel asosidagi payvandlash simi ishlatiladi. Bunga B160 - B163, B725 va B730 kabi ASTM sinflari kiradi.
· Nikel qotishmalaridan zanglamaydigan yoki ferritli po'latlarga qadar turli xil qo'llanmalarda qo'llaniladi.
· Uglerodli po'latni qoplash va quyma temir quymalarni ta'mirlash uchun ishlatiladi.
150 0000 2421