Baho | 0Cr27Al7MO2 |
Hajmi | 0,1-1,2 mm |
Yuzaki | yorqin tavlangan |
Og'irligi | 1-3 kg / rulo |
Qarshilik | 1,53±0,07mk.m |
Eng yuqori harorat | 1400 ℃ |
Zichlik | 7,1 g/sm³ |
Mustahkamlik chegarasi | 750N/mm² |
Cho'zilish | ≥10% |
Mahsulot parametrlari
Baho | Eng yuqori harorat | Qarshilik | Erish nuqtasi | Mustahkamlik chegarasi | Cho'zilish |
0Cr21Al4 | 1100 ℃ | 1,23±0,06mŌ.m | 1500 ℃ | 750 | ≥12 |
0Cr25Al5 | 1250 ℃ | 1,42±0,07mk.m | 1500 ℃ | 750 | ≥12 |
0Cr23Al5 | 1300 ℃ | 1,35±0,06mk.m | 1500 ℃ | 750 | ≥12 |
0Cr21Al6NbCo | 1350 ℃ | 1,43±0,07mk.m | 1510 ℃ | 750 | ≥12 |
0Cr27Al7Mo2 | 1400 ℃ | 1,53±0,07mk.m | 1520 ℃ | 750 | ≥10 |
KSC | 1350 ℃ | 1,44±0,05mk.m | 1510 ℃ | 750 | ≥16 |
Cr20Ni80 | 1200 ℃ | 1,09±0,05mk.m | 1400 ℃ | 750 | ≥20 |
Cr15Ni60 | 1150 ℃ | 1,12±0,05mk.m | 1390 ℃ | 750 | ≥20 |
Cr20Ni35 | 1100 ℃ | 1,04±0,05mk.m | 1390 ℃ | 750 | ≥20 |
Cr20Ni30 | 1100 ℃ | 1,04±0,05mk.m | 1390 ℃ | 750 | ≥20 |
Baho | Kimyoviy tarkibi% | ||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | |
≤ | |||||||||
0Cr21Al4 | 0,12 | 0,025 | 0,025 | 0,7 | ≤1,0 | 17-21 | ≤0,6 | 3-4 | muvozanat |
0Cr25Al5 | 0,06 | 0,025 | 0,02 | 0,5 | ≤0,6 | 23-26 | ≤0,6 | 4,5-6,5 | muvozanat |
0Cr23Al5 | 0,06 | 0,025 | 0,02 | 0,5 | ≤0,6 | 20,5-23,5 | ≤0,6 | 4.2-5.3 | muvozanat |
0Cr21Al6Nb | 0,05 | 0,025 | 0,02 | 0,5 | ≤0,6 | 21-23 | ≤0,6 | 5-7 | muvozanat |
0Cr27Al7Mo2 | 0,05 | 0,025 | 0,02 | 0.2 | ≤0,4 | 26,5-27,8 | ≤0,6 | 6-7 | muvozanat |
Cr20Ni80 | 0,08 | 0,02 | 0,015 | 0,6 | 0,75-1,6 | 20-23 | muvozanat | <0,5 | ≤1,0 |
Cr15Ni60 | 0,08 | 0,02 | 0,015 | 0,6 | 0,75-1,6 | 15-18 | 55-61 | <0,5 | muvozanat |
Cr20Ni35 | 0,08 | 0,02 | 0,015 | 1.0 | 1-3 | 18-21 | 34-37 | - | muvozanat |
Cr20Ni30 | 0,08 | 0,02 | 0,015 | 1.0 | 1-3 | 18-21 | 30-34 | - | muvozanat |