Inconel 600 yuqori nikel qotishma varag'i/lenta nichromga chidamlilik tasmasi
ASTM B603, DIN 17470, JIS C2520, GB/T1234.
Bizning afzalligimiz: Yuqori sifat, qisqa yetkazib berish muddati, kichik MOQ.
Xususiyatlari: Barqaror ishlash; Oksidlanishga qarshi; Korroziyaga chidamlilik; Yuqori harorat barqarorligi; Zo'r spiral hosil qilish qobiliyati; Dog'larsiz bir tekis va chiroyli sirt holati.
Foydalanish: Qarshilik isitish elementlari; Metallurgiyadagi materiallar; Maishiy texnika; Mexanik ishlab chiqarish va boshqa sohalar.
| Baho | Ni80Cr20 | Ni70Cr30 | Ni60Cr23 | Ni60Cr15 | Ni35Cr20 | Karma | Evanohm | |
| Nominal tarkib% | Ni | Bal | Bal | 58.0-63.0 | 55.0-61.0 | 34.0-37.0 | Bal | Bal |
| Cr | 20.0-23.0 | 28.0-31.0 | 21.0-25.0 | 15.0-18.0 | 18.0-21.0 | 19.0-21.5 | 19.0-21.5 | |
| Fe | ≦1.0 | ≦1.0 | Bal | Bal | Bal | 2.0-3.0 | – | |
| Al1.0-1.7 Ti 0.3-0.5 | Al2.7-3.2 Mn0.5-1.5 | Al2,7-3,2 Cu2,0-3,0 Mn0,5-1,5 | ||||||
| Maksimal ish harorati (°C) | 1200 | 1250 | 1150 | 1150 | 1100 | 300 | 400 | |
| Qarshilik (Ω/smf, 20℃) | 1.09 | 1.18 | 1.21 | 1.11 | 1.04 | 1.33 | 1.33 | |
| Qarshilik (uΩ/m, 60°F) | 655 | 704 | 727 | 668 | 626 | 800 | 800 | |
| Zichlik (g/sm³) | 8.4 | 8.1 | 8.4 | 8.2 | 7.9 | 8.1 | 8.1 | |
| Issiqlik o'tkazuvchanligi (KJ/m·h·℃) | 60.3 | 45.2 | 45.2 | 45.2 | 43.8 | 46.0 | 46.0 | |
| Chiziqli kengayish koeffitsienti(×10¯6/℃)20-1000℃) | 18.0 | 17.0 | 17.0 | 17.0 | 19.0 | - | - | |
| Erish nuqtasi (℃) | 1400 | 1380-yil | 1370-yil | 1390-yil | 1390-yil | 1400 | 1400 | |
| Qattiqlik (Hv) | 180 | 185 | 185 | 180 | 180 | 180 | 180 | |
| Cho'zilish kuchi (N/mm)2 ) | 750 | 875 | 800 | 750 | 750 | 780 | 780 | |
| Uzayish (%) | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | 10-20 | 10-20 | |
| Mikrografik tuzilish | ostenit | ostenit | ostenit | ostenit | ostenit | ostenit | ostenit | |
| MagneticProperty | Yo'q | Yo'q | Yo'q | Biroz | Yo'q | Yo'q | Yo'q | |
| Tez hayot (soat/℃) | ≥81/1200 | ≥50/1250 | ≥81/1200 | ≥81/1200 | ≥81/1200 | - | - | |