Kimyoviy tarkibi
Baho | Ni% | Cu% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
Monel K500 | Min 63 | 27,0-33,0 | 2.30-3.15 | 0,35-0,85 | Maks 2.0 | Maksimal 1,5 | Maksimal 0,01 | Maksimal 0,25 | Maksimal 0,5 |
Texnik xususiyatlari
Shakl | Standart |
Monel K-500 | UNS N05500 |
Bar | ASTM B865 |
Tel | AMS4676 |
Choyshab/plastinka | ASTM B865 |
Soxtalashtirish | ASTM B564 |
Payvandlash simi | ERNiCu-7 |
Jismoniy xususiyatlar(20°C)
Baho | Zichlik | Erish nuqtasi | Elektr qarshiligi | Issiqlik kengayishining o'rtacha koeffitsienti | Issiqlik o'tkazuvchanligi | Maxsus issiqlik |
Monel K500 | 8,55 g/sm3 | 1315 ° C-1350 ° S | 0,615 mk•m | 13,7(100°C) a/10-6°C-1 | 19,4(100°C) l/(Vt/m•°C) | 418 J/kg•°C |
Mexanik xususiyatlar(20°C min)
Monel K-500 | Mustahkamlik chegarasi | Hosildorlik kuchi RP0,2% | Cho'zilish A5% |
Tavlangan va qarigan | Min. 896 MPa | Min. 586 MPa | 30-20 |
Oldingi: Avtomobil/avtomobil o'rindiqlarini isitish uchun mo'ljallangan emallangan mis sim CuNi6 ishlab chiqaring Keyingisi: Rezistor qo'rg'oshin uchun 20 AWG sirlangan payvandlash qalaylangan mis sim